Laser stitching is done by using a laser drill and drilling vias from the
layer 1 to 2 about 1 cm or less apart in a stitching pattern. I am
interested in knowing the reason for doing this.
Thank you
----- Original Message -----
From: <[log in to unmask]>
To: <[log in to unmask]>; <[log in to unmask]>
Cc: <[log in to unmask]>
Sent: Tuesday, December 14, 2004 11:00 AM
Subject: Re: [TN] Laser Stitching
> Hi Scott - can you better define "Laser stitching" please (do you mean
> soldering or welding or brazing?).
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
>
>
> "Scott B.
> Westheimer"
> <swestheimer@HOTM To
> AIL.COM> [log in to unmask]
> Sent by: TechNet cc
> <[log in to unmask]>
> Subject
> [TN] Laser Stitching
> 12/14/2004 09:50
> AM
>
>
> Please respond to
> TechNet E-Mail
> Forum
> <[log in to unmask]>
> ; Please respond
> to
> "Scott B.
> Westheimer"
> <swestheimer@HOTM
> AIL.COM>
>
>
>
>
>
>
> Can someone tell me where I might find an article and/or information on
> Laser stitching.
>
> Thank you
> Scott B. Westheimer
> 5709 Clarks Fork Drive
> Raleigh, N.C. 27616
> Phone: (919)713-0748
> Office: (919)713-4258
> Cell: (919)961-5364
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
> Email: [log in to unmask]
>
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------