Yep... Joyce points out your biggest headache. Most CM's profit margins
are heavily determined by how they manage material inventories. Since
many (if not most) components will become available in "only" lead-free
packages, your "leaded" customers will not be able to complete their
BOM's in a few years time. (Check your caps and resistors...few remain
leaded)
So now it's a gamble! Will xxxx component become lead-free only so buy
now? Will supply and demand make the leaded components scarce thus
higher priced, so buy now, or buy in a year, maybe two years? Buy a lot
and end up with inventory that you can't move? Not buy enough and be
unable to complete an order? Maybe you can get your customer to pay for
the future parts now?
We had many server customers tell us the same thing. Leaded only. Of
course we bucked up and said "Yes Sir!". Hence the dual leaded and
leadfree processes. However, they have eased up on the militant - no
lead-free components - once the sales team was informed by purchasing
that such and such BOM can never be built again because xxxx leaded
component no longer exist as leaded! ALL of them (customers) agreed to
allow the lead-free components, provided they are not BGA. (What else
could they say...That they won't sell their product just to spite the
component industry?) However, some still insist on leaded solder paste.
I feel for you Steve...I don't envy any CM.
Ryan
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joyce Koo
Sent: Monday, December 06, 2004 1:02 PM
To: [log in to unmask]
Subject: Re: [TN] Lead-free, and not lead-free...
Steve,
"I envision that we will be building tin/lead products for quite a few
years
yet. Military minds don't change easily. Besides, there are exemptions
for
defense related electronics"
if you follow Mike's advice, you will do no wrong ;-).
As for the mil-mind, it is driven by all the obsolesces parts from
commercial supply. The few years back, few of the chip supplies cancel
many
of their part numbers due to either (a) change to large wafer format, or
(b)
limited demand = few thousand aircrafts vs. million of commercial
electronics. That leave the assembly producer with little choice: (a)
re-spin the whole board with new "hi-rel commercial device with
up-grating",
normally you need re-qual of the assembly, or (b) do a life time buy of
the
parts and stored in N2 or any way you know how to keep the aircraft
going
(life time of the mil-aircraft is much longer than the 3-5 years of
commercial electronics). Most of the so call "life time =last time
buying
parts are lead/tin finishing. (some of them are gold finishing, so you
can
store longer and tin them as you required.. those are ASICs, FPGAs, and
microprocessors... large device size, so you do not have to worry too
much
about rad-hardening). most of the assemblies are try to keep the parts
list
compatible to each other, so you can buy "large qty", the qty still very
very small compare to the commercial lot.
If you start introduce leadfree, look like you will have to re-spin the
board and re-qual at assembly level, if not at system level (I am sure
those
are new generation of devices, that is possibly sub-micron metallization
for
VLSI, if you are lucky... otherwise, you are dealing with ULSI. if it is
really state of the art generation devices. As for new design, it
should
not be an issue. But the device selection will be limited at current
level
(after few years, it may be different). You are caught at rock and hard
places...
jk my 1.66 cents
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Steve Gregory
Sent: Monday, December 06, 2004 2:02 PM
To: [log in to unmask]
Subject: Re: [TN] Lead-free, and not lead-free...
Hi Ryan!
Unfortunately, this isn't going to be a transitional thing for me, at
least
in the near future anyway. We're a contract assembly company that builds
things for most of the the major DoD contractors, and most of them have
told
me informally that they aren't even thinking about lead-free. Some have
actually put it into writing. I've pasted a few paragraphs as an example
that was sent to us recently below (I've blanked out the company name:
"At present, (Blank) will continue to order and assemble electronic
products
using tin-lead solder. There are currently no (Blank)customer contracts
requiring transition to lead-free solders.
There are, however, (Blank) customer contract requirements for (Blank)
to
continue using lead-based solders. These requirements are currently
driven
by a lack of community acceptance of reliability and design data to
safely
transition to lead-free solders.
We are also concerned about our ability to guarantee the life of
products,
and our lack of process controls within (Blank)to manufacture with
lead-free
components.
If there is a change in position, (Blank) will notify our suppliers of
any
new requirements. Presently, (Blank) is requesting that all suppliers
provide lead-based electrical components and assemblies to (Blank) on
all
orders.
(Blank)is monitoring industry work/study group efforts involved in
lead-free
solder transition, and while much still needs to be done, we are also
establishing an internal program to evaluate transitioning to lead-free
electronic assemblies, if and when that time comes."
So, I have that stance from existing customers, and have just learned
that
we are pursuing business with a company that will have their products
marketed in the EU, and must comply with WEEE and RoHS. So I find myself
in
quite a "pickle", as it were...
I envision that we will be building tin/lead products for quite a few
years
yet. Military minds don't change easily. Besides, there are exemptions
for
defense related electronics.
But if we're going to be build lead-free stuff along with tin/lead
stuff,
I'm inclined to agree with Mike Fenner and set-up completely separate
areas
with an impenetrable wall between them ;^)
-Steve Gregory-
Hi Steve,
We're doing it no sweat! :) O.K., just kidding. Actually, it hasn't
been
too bad, we require our solder paste suppliers to visually mark their
tubes
with a "green" color so they aren't easily mixed.
(Snip...)
That would be easier to replace the eventually contaminated pot and keep
pure. Ideally, you would convert all wave solder machines to lead-free,
assuming all your leaded customers agree to the change. Then the only
risk
is production operators using the wrong solder paste.
Good luck on the conversion.
Ryan Grant
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Saturday, December 04, 2004 6:21 PM
To: [log in to unmask]
Subject: [TN] Lead-free, and not lead-free...
Hi All!
I've got a problem that I've been worrying about all weekend. It may
come to
pass that we will be building both lead-free, and standard 63/37
stuff...whoa is me.
I'm interested in stories from those that have done that...what the hell
did
you do?
Is this something that can be done? It probably can, but me, being the
pessimistic sort, thinks that you're just asking for trouble when you
try to
mix the two...
-Steve Gregory
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|