I think this was actually covered by Adam and Jamie on Mythbusters. As
I remember they put a dead pig in concrete and yes it did decompose and
leave a pig shaped void in the concrete.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Thomas Bauer
(Venture-USA)
Sent: Thursday, December 23, 2004 1:12 PM
To: [log in to unmask]
Subject: [TN] NTC: Friday type question
Here is a question to ponder over for this Friday type day. Yes, Jimmy
Hoffa was in the discussion.
If a human body was to be placed in a bed of curing concrete, would the
body decompose? If the entire body is encased in the middle of said
concrete that is say 4 sq ft thick on all sides, would there be any
microscopic deterioration or would the little critters still infiltrate
and do there "thing"? This was just a casual discussion amongst
co-workers so I thought it would be a good Friday question. Any takers?
Oh, if the body did fully decompose, would the structural integrity of
the concrete be affected?
Thomas Bauer
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|