TECHNET Archives

December 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>
Date:
Mon, 13 Dec 2004 08:40:52 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Brooks,Bill" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Brooks,Bill" <[log in to unmask]>
Parts/Attachments:
text/plain (136 lines)
This is indeed an interesting subject... 

Is it possible that the production of water through combustion of oxygen and
hydrogen would be more pure and lack all the dissolved solids that are in
water that has passed through the atmosphere as rain or of course water that
has dissolved solids in it from the ground, or worse yet the slat water in
the oceans. Would that be more economical than filtering and deionizing and
treating the water with UV? Don't the 'fuel cells' they use on the space
shuttle use a similar catalytic action to create electricity from hydrogen? 
I wonder if that might be a more economical way to produce pure water than
with the current methods...

Best regards,


Bill Brooks - KG6VVP
PCB Design Engineer , C.I.D.+, C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
e-mail:[log in to unmask]
http://www.dtwc.com
http://pcbwizards.com

-----Original Message-----
From: Brian Ellis [mailto:[log in to unmask]] 
Sent: Tuesday, December 07, 2004 11:00 PM
To: [log in to unmask]
Subject: Re: [TN] DI Water

Let me add my CYP 0.02 worth. If you take potable tap water, pass it 
through a new mixed bed DI column, and drink it, it will not harm you in 
any way. It'll taste bloody 'orrible, but that's another story.

If you do the same with a column that's been in service for some time, 
then there is a risk of excess micro-organisms of unknown species having 
proliferated in the resin bed. I've seen DI columns in clear plastic 
tubes turn green with algae and the chlorination of tap water does not 
prevent it. Probably the same applies to some bacteria, a few of which 
may be harmful.

I disagree with the guy who said that DI water could not be better than 
2 megohm-cm. Let me quote facts:
1. RO does not deionise: it removes all dissolved impurities by a factor 
of about 10 to 20. If your water starts with a conductivity of, say, 300 
µS-cm (typical for a medium quality tap water), it'll have a 
conductivity of 15 - 30 µS-cm after a single RO stage and non-ionic 
dissolved material will also be removed in about the same proportions. 
To prepare potable water from sea water in a desalination plant, it will 
require two- to three-stage desalination, UV microorganism murder and 
remineralisation.
2. Distillation is not a very effective way of purification, despite 
popular belief. It, too, will only remove dissolved solids by a factor 
of about 50 to 100 per stage. This is explained by the fact that boiling 
water produced bursting bubbles on the surface and these throw minute 
droplets of water + impurities into the steam. The water in these 
droplets evaporates and the impurities float around as an aerosol and 
get partially washed out by the condensate. In addition, the 
constructional materials of the still tend to dissolve slowly in the 
distillate. The distillate will also pick up CO2 from the air if it is 
allowed to trickle into the receiver. Even triple distilled in quartz 
water, which is the purest you will find, will rarely have a 
conductivity better than 0.2 to 0.5 µS-cm and is usually complemented by 
a mixed bed DI column to bring it down to typically 0.06 µS-cm 
(so-called "18 megohm" water). Distillation is horribly energy-intensive.
3. DI water produced by simply passing tap water through separate cation 
and anion beds, followed by a "polishing" mixed bed DI column will have 
a conductivity as low as 0.06 µS-cm but will still have almost its full 
complement of non-ionic dissolved solids. If subsequently passed through 
two carbon columns (different adsorption characteristics) and UV 
irradiation, followed by a 0.1 µm mechanical filter, it will be 
practically the same as the purest "18 megohm" water. This is what is 
used for semiconductor production, except that it is preceded by a 
single stage RO, as well.

Brian

David Tremmel wrote:
> Dear Technetters,
> 
> As a joke, someone asked me what would happen if they drank DI water and
it
> started me thinking.  Is DI Water potable?
> 
> Thank you,
> 
> David Tremmel
> Belmont Trading
> 3160 MacArthur Boulevard
> Northbrook, IL 60062
> (847) 412-9690, Ext. 345
> (847) 858-5540, Cellphone
> 
> _________________________________________________________________
> ¿Cuánto vale tu auto? Tips para mantener tu carro. ¡De todo en MSN Latino
> Autos! http://latino.msn.com/autos/
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site 
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional 
> information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 
> ext.2815
> -----------------------------------------------------
> 
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2