Frank:
I know of board shops that swear by the Perfect Test system. These tend to
be larger companies that have the resources to throw at it. Some
consideration:
-You have to give up some real estate on the panel to place the coupon.
-You will be adding on a fair amount of drill hits
-You will have to read and analyse the data
-You will have to put this back into CAM to adjust scaling.
This should all be a closed loop system
One company I heard of in the Northeast (No longer in business) had
registration dialed in for every layup; including panel size, core thickness
and even the prepreg used against the core.
I think most companies, if they add this coupon to the panel, program the
coupon seprately so they can turn off the coupon when the panel is in
production. (after testing)l
There are a number of these systems available through used equipment
dealers.
Good Luck,
pete
>From: Franklin D Asbell <[log in to unmask]>
>Reply-To: TechNet E-Mail Forum <[log in to unmask]>, Franklin D
>Asbell <[log in to unmask]>
>To: [log in to unmask]
>Subject: [TN] PerfectTest registration control system
>Date: Tue, 21 Dec 2004 12:14:10 -0600
>
>Is anyone out there familiar with the PerfectTest registration control
>system? If so how would yo rate it?
>
>As we evolve into tighter space/trace features including annular ring,
>vias, bga etc etc we are looking for better controls for registration and I
>found the system identified above, was wondering what other shops are using
>for process control, testing or inspection of registration, other control
>methods, materials, etc etc etc...
>
>Thanks,
>
>
>---------------------------------------------------
>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt or (re-start) delivery of Technet send e-mail to
>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search the archives of previous posts at: http://listserv.ipc.org/archives
>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>for additional information, or contact Keach Sasamori at [log in to unmask] or
>847-615-7100 ext.2815
>-----------------------------------------------------
>Franklin
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|