TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Scott B. Westheimer" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Scott B. Westheimer
Date:
Thu, 4 Nov 2004 18:43:17 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (54 lines)
The void seems to be in the center of the hole and circular. This is
normally caused by air entrapment during the electro copper process after
drilling. However, most of the time the voiding due to these is larger so it
is possible that there was a thermal cycle was performed prior to tin and
the board expanded and fractured. The picture is not that clear. I do not
see a lot of roughness due to drilling so I would assume that it is due to
air entrapment and I would ask the supplier why it was not caught during
electrical test
----- Original Message -----
From: "Al Onderick" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Thursday, November 04, 2004 5:55 PM
Subject: [TN] Via hole failures (with pictures)


>I have a couple of boards that have failed at a customer site. After
> testing, a via was identified as open. The following link is a picture of
> the cross section.
>
> http://www.tier1gear.com/temp/via_crack.jpg
>
> The board was .062, the via .010 and the surface finish immersion white
> tin.
>
> I would appreciate any insight into what may cause a failure like this.
>
> Al Onderick
> National Instruments
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2