Mainly I am looking for your opinion on quality related issues when
compared to Vertical Desmear Line with Horizontal Desmear Line.
Best regards,
Raghavendra Rao
Colin McVean
<cmcvean@CIRCUITM To: [log in to unmask]
AN.CO.UK> cc:
Sent by: TechNet Subject: Re: [TN] Desmear Line
<[log in to unmask]>
10/28/04 09:08 PM
Please respond to
TechNet E-Mail
Forum; Please
respond to Colin
McVean
Vertical lines can also be automated
<When you discuss horizontal vs. vertical, you mean conveyorized vs. a
tank
line?
A horizontal (conveyorized) line will cost much more, and take up much more
floor space, than a vertical (tank) line, for the same production per hour.
Also, a vertical line must be manually loaded and unloaded, whereas
horizontal lines can be made to be automatically load, and unload.
Rudy Sedlak
RD Chemical Company>
Regards,
Colin McVean
Circuit Manufacture Ltd
Unit 9-12
Rowleys Green Lane
Longford
Coventry
CV6 6AG
Tel: 02476 666168
Fax: 02476 637089
________________________________________________
This email is confidential and intended solely for the use
of the individual to whom it is addressed. Any views or
opinions presented are solely those of the author and do
not necessarily represent those of the Company.
If you are not the intended recipient, be advised that you
have received this email in error and that any use,
dissemination, forwarding, printing, or copying of this
email is strictly prohibited.
If you have received this email in error please notify the
Company by telephone on +44 (0)24 7666 6168 or reply
by email to the sender and delete the email.
________________________________________________
Whilst every effort has been made to ensure that there are
no viruses embedded in this email, we highly recommend
that you virus scan any attached files using your own anti-
virus software.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of R Sedlak
Sent: 28 October 2004 16:25
To: [log in to unmask]
Subject: Re: [TN] Desmear Line
When you discuss horizontal vs. vertical, you mean conveyorized vs. a tank
line?
A horizontal (conveyorized) line will cost much more, and take up much more
floor space, than a vertical (tank) line, for the same production per hour.
Also, a vertical line must be manually loaded and unloaded, whereas
horizontal lines can be made to be automatically load, and unload.
Rudy Sedlak
RD Chemical Company
[log in to unmask] wrote:
Dear Technetters,
Can anybody share the advantages and disadvantages of horizontal and
vertical desmear lines. Which is the preferred one?
Thanks for your valuable suggestions.
Best regards,
Raghavendra Rao
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Y! Messenger - Communicate in real time. Download now.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|