Eric:
You cannot get anywhere near the specified thickness with immersion Silver, that said, you may not need to, as immersion Silver probably has a significantly longer shelf life than ED Silver, as it contains a nice load of antitarnish co-deposited with the silver.
Rudy Sedlak
RD Chemical Company
Eric Kalgren <[log in to unmask]> wrote:
Good morning TechNet,
One of our drawings for an RF PCB calls out "Silver Plate per QQ-S-365,
electrodeposited, Type I, 0.0003" thk." The supplier that we are
getting quotes from says he can't do electrodeposit and wants to supply
immersion silver boards.
Are these two processes equivalent? I searched the archives and cannot
find any references to ED silver. Has immersion replaced this process?
(Our drawing is pretty old.)
The board material is Duroid 5880. would this make a difference?
Thanks for your help!
Eric Kalgren
Manufacturing Engineer
Atlantic Microwave
Phone: 978-779-7062
Fax: 978-779-0101
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
Do you Yahoo!?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Check out the new Yahoo! Front Page. www.yahoo.com
|
|
|