You know with all puns set aside it was probably a fruit fly that was in
the wrong place at the wrong time. When they did the solder mask I would
assume it was screened on? The little bugger was in the way and became
part of your circuit. I guess this puts a fly in your ointment when it
comes to debugging this board.
Steve Gregory
<[log in to unmask] To: [log in to unmask]
M> cc:
Sent by: TechNet Subject: [TN] Strange Soldermask Defect...
<[log in to unmask]>
11/16/04 03:41 PM
Please respond to
TechNet E-Mail
Forum; Please
respond to
SteveZeva
Hi All!
Well, I've run across some strange problems in my time, but this one is a
new one to me.
I was on the production floor just after lunch, close by one of our final
inspectors looking at something under her microscope, when I hear her say;
"What the heck is this?" then I hear this big; "EWWWWWW!" from her...
"Steve! Steve! You gotta' look at this!" she says to me. I pull up a chair
and peer into the microscope, and I have to say, I've never, ever seen this
before.
Take a look at:
http://www.stevezeva.homestead.com/files/StrangeMaskDefect.jpg
and
http://www.stevezeva.homestead.com/files/StrangeMaskDefectCloseUp.jpg
What should I do? Should I send this to a lab or something? I don't know
what to tell my inspectors, much less explain this to our customer...this
really tops my list as one of the strangest defects I have ever seen.
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
STATEMENT OF CONFIDENTIALITY:
If you have received this e-mail in error, please immediately notify the
sender by e-mail at the address shown. This e-mail and any attachments may
contain confidential information. This information is intended only for the
use of the individual(s) or entity to whom it is intended even if addressed
incorrectly. Please delete it from your files if you are not the intended
recipient. Thank you for your compliance.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|