Reuven
I installed the first immersion silver line in North American at the
AT&T PCB facility in 95. It was a great success with the customers, in
particular Lucent. All that I have experienced since then has been very
positive.
Several papers have been published other than my own on immersion
silver. The two I would suggest are the paper by George Wenger and Bob
Furrow at Lucent and the IPC study comparing several metallic finishes.
The second was prepared by and IPC committee chaired by Bruce Haughton
of Celestica.
Best regards
Lee
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Reuven ROKAH
Sent: Sunday, November 14, 2004 4:10 AM
To: [log in to unmask]
Subject: [LF] Immersion Silver vs Immersion Tin (whiskers free)
Hello All,
Pls inform if you have work / experience / test report / comparison
table
on the above issue.
Best Regards
Reuven ROKAH
------------------------------------------------------------------------
-------Leadfee Mail List provided as a service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks
send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
-------
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|