I have a customer asking for Imm Silver over 100um NI. I am concerned putting the Silver over the NI as it may lift or peel. This is the first time I have had this kind of request. Have any of you well informed Tech Heads heard of this before???
ps. This customer also asked for OSP over the Silver over the NI. I KNOW that is not done.