I know if I were a Bobcat and they took my mate away, I wouldn't work
either.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bob willis
Sent: Monday, November 29, 2004 12:40 PM
To: [log in to unmask]
Subject: Re: [TN] Die Penetrant SJ Crack Inspection Process
For some reason the email forum software Listserve has split up the links,
that is why they don't work. It may be set to not accept spaces. We use the
same software for smart-e-link the SMART Group Forum. Hope the links are OK
in the Word document, can't send the list to the Forum.
Many thanks
Bob Willis
2 Fourth Ave, Chelmsford,
Essex, CM1 4HA, England
Tel: 01245 351502
Fax: 01245 496123
Mobile: 07860 775858
Email: [log in to unmask]
Web: www.leadfreesoldering.com
Web: www.bobwillis.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Judy Rae Brown
Sent: 29 November 2004 19:31
To: [log in to unmask]
Subject: Re: [TN] Die Penetrant SJ Crack Inspection Process
none of the links work
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Bob willis
Sent: Monday, November 29, 2004 11:14 AM
To: [log in to unmask]
Subject: Re: [TN] Die Penetrant SJ Crack Inspection Process
Here is a link to a short paper on dye testing, don't get on your fingers as
its stays red or yellow for a few days.
www.bobwillis.co.uk/guide/BGA Dye Testing.pdf
Also the guy at Universal Instruments did a couple of good papers as well.
There are a few more links as well.
www.bobwillis.co.uk/guide/VP Soldering Lead Free.pdf
www.bobwillis.co.uk/guide/0201 Design Assembly.pdf
www.bobwillis.co.uk/guide/Component Cleaning Tests.pdf
www.bobwillis.co.uk/guide/Lead Free Component Requirements.pdf
www.bobwillis.co.uk/guide/PCB Pad Design.pdf
www.bobwillis.co.uk/guide/PPM DPMO Monitoring your Process.pdf
www.bobwillis.co.uk/guide/Solder Beading.pdf
Bob Willis
2 Fourth Ave, Chelmsford,
Essex, CM1 4HA, England
Tel: 01245 351502
Fax: 01245 496123
Mobile: 07860 775858
Email: [log in to unmask]
Web: www.leadfreesoldering.com
Web: www.bobwillis.co.uk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Newland, Scott
Sent: 29 November 2004 15:56
To: [log in to unmask]
Subject: [TN] Die Penetrant SJ Crack Inspection Process
I'm going to be performing some long duration thermal cycling testing on
some
CGA components that will not be electronically monitored for opens. This is
not
my preferred approach, but a reasonable daisy chain test component was not
available. My current plan is to periodically remove parts and cross
section
the outside rows. I also wanted to try using die penetrant to inspect for
SJ
cracks. As I understand the process you flooding the SJ under the part with
Die
penetrant, clean, then pull the parts off vertically, and inspect for
pre-existing cracks marked by the die.
Is the die penetrant inspection worth while? Does anyone have or know of a
written procedure for using die penetrant to inspect for SJ cracks? Any
other
suggestions for identifying the "needle in the hay stack" cracks?
Scott Newland
Harris GSCD
321 727 6472
Pager 321 690 4131
E-Mail [log in to unmask]
For a brain teaser try:
http://pao.gsfc.nasa.gov/science.html
This information is only intended for the use of the individual or entity
named
in this email. If you are not the intended recipient, you are hereby
notified
that any disclosure, copying, distribution, or use of the contents of this
information is strictly prohibited. If you have received this email in
error,
please notify me and delete it immediately.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|