That story is a little hard to Swallow.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Franklin D Asbell
Sent: Tuesday, November 16, 2004 3:00 PM
To: [log in to unmask]
Subject: Re: [TN] Strange Soldermask Defect...
I went into a plating shop years ago, this shop had open bay doors on both
sides to vent the place, so it attracted all sorts of "stuff" that probably
should not be there...as I pass a silver plating bath the operator is
scooping what they called "contaminates" from the bath...he was using a
screen similar to those the pool service guys use...and I noticed him scoop
up and throw in a bucket...a small bird...(chuckle)...I was not quite sure
how to document that in the audit report I was completing...would that be
organic contaminates??? and how many PPM sparrow are allowed in a cyanide
silver bath???
Someone needs to write a book about these strange and unusuals...market it
of course as comedy...
Franklin
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|