1oz/sq.ft. = 0.0014" = 35µm cu thickness
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Joe Spicuzza
Sent: Thursday, November 04, 2004 5:02 PM
To: [log in to unmask]
Subject: [TN] copper weight
Greetings fellow technetters!
I have a German customer who would like to convert the standard; 1 oz., 2 oz. copper on their drawings into the metric system, specifically microns. Does anyone know of a conversion table or just the conversion factor one would use. I'm thinking that say 1 oz./ sq.ft. would become some grams per micron, but have been told it's not that simple. Help!
Joseph Spicuzza
Production Manager
Millennia Technology, Inc.
1105 Pittsburgh Street
Cheswick, PA 15024
724 274-2222 PHONE
724 274-2235 FAX
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
======================================================================
This electronic message transmission and any attachments are
confidential and may constitute legally privileged information of
Bioveris Corporation. The information is intended for solely
the use of recipient (recipient). If you are not
the intended recipient, you are hereby notified that any
disclosure, copying, distribution or the taking of any action in
reliance of this information is strictly prohibited. You are not
authorized to retain it in any form nor to re-transmit it, and
you should destroy this email immediately.
If you have received this electronic transmission in error,
please notify us by telephone (800-336-4436) or by electronic
mail to the sender of this email, Thomas, Brian ([log in to unmask]),
immediately.
=====================================================================
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|