TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 25 Nov 2004 04:42:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Hughes, Chris" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Hughes, Chris" <[log in to unmask]>
Parts/Attachments:
text/plain (150 lines)
OK so there seems to be a decent amount of conversation & discussion about lead free. 

Let me ask this, how many of you are prepared to meet the requirements of the forthcoming WEEE & RoHS Directives?

By changing over to lead-free, doesn't necessarily mean your products will be compliant, and permitted for sale in the EU after 1 July 2006.

Lead is only one(1) of six(6) substances that will be heavily restricted for incorporation in electronic and electrical equipment sold in the EU after July 1 2006. Bottom line is if you can't prove your compliance with WEEE & RoHS, your customers will seek alternative suppliers who can. Why? Because the risk of incorporating components/materials within their products that they cannot be sure is compliant is too large. Their products could be banned from sale in the EU, and they could be fined.

Some advice I will share with you all following a discussion I had with one of our clients marketing people: Do not satisfy your customer's declarations of conformity requests, and deal with the issues later. This is very risky, and could easily come back to haunt you. Think of the time between your customers ordering from yourselves, to the final product with your component/materials incorporated within, going to the end-user. Lag periods can be anything from 3 months to 2 years.

The most common questions we get are, what are the WEEE & RoHS Directives, and how do they effect our organisation??

Or, we are only concerned about lead, and we have only issues with lead. This is risky, how do you know none of your cabling, flux etc, doesn't contain any of the 6 banned substances? Have you had every material you use analysed? Or are you only taking your suppliers word for it? 

Please think about the bigger picture, and feel free to e-mail me off line if you want to discuss any issues surrounding the WEEE & RoHS Directives...

Chris

Christopher Hughes
Environmental Scientist 
[log in to unmask] 
 


-----Original Message-----
From: James Hofer [mailto:[log in to unmask]] 
Sent: 24 November 2004 21:33
To: [log in to unmask]
Subject: Re: [TN] FR4 and Lead free

We have many customers requesting lead free materials. We use a specific
material with a higher Td which is specifically designed for lead free and
is widely used in Asia where the lead free initiative is much further along.

Our lead free material is actually less expensive than the current "dicey"
cured materials we use for non lead free assemblies.

If you want more information please feel free to contact me off-line.

James Hofer
Director of Operations
Accurate Circuit Engineering
3019 S. Kilson Dr.
Santa Ana Ca. 92707-4202
714-546-2162 work
714-473-6127 cell
[log in to unmask]
----- Original Message -----
From: "Jeffrey Bush" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, November 24, 2004 12:34 PM
Subject: Re: [TN] FR4 and Lead free


The issue is not Tg but Td.  Some higher Tg materials actually perform
worse than lower Tg materials.  It is important develop a test program
to validate your lead free process with specific base materials.
Laminate manufactures offer some variety of thermally stable materials
targeting lead-free, but these are used at a premium.  If your lead-free
process can be supported by existing base materials, than that is best
economic solution.  The test program will provide the feedback needed.

Please contact me off-line if you need specific information on alternate
base materials and Td for lead-free.

Jeffrey Bush
Director, Quality Assurance and Technical Support

VERMONT CIRCUITS INCORPORATED
  76 Technology Drive - POB 1890
    Brattleboro, Vermont 05302
      Voice: 802.257.4571.21 Fax: 802.257.0011
           http://www.vtcircuits.com


-----Original Message-----
From: Black, Paul [mailto:[log in to unmask]]
Sent: Wednesday, November 24, 2004 3:08 PM
To: [log in to unmask]
Subject: [TN] FR4 and Lead free

Hi Tech Gurus,

As people talk more and more about Lead free, I keep hearing that
standard FR boards might not be able to take the extra heat required for
a reliable Lead free solder joint. The problem is that I keep hearing
the word MIGHT. I have not heard that this is definitely true and, if it
is true, I have not heard anyone offer a cost effective solution. So, I
am asking the many experts on this forum, will standard FR4 be able to
handle the higher excursions (particularly, let's say, for a 7" X 9",  8
layer, double-sided SMT, .062" 5/5 board) associated with Lead free
solder paste? If not, what would be the most cost-effective offering
(i.e. high Tg FR4)?

Thank you,
Paul Black
Manufacturing Engineer
Kronos

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2