My guess is your PCB FAB shop has ENIG and is trying to sell you what he has to offer. If you ask a PCB FAB shop that has IAg they will probably try to tell you ENIG is more expensive than IAg and you won't get Black Pad failures from IAg. My advice is to ask a PCB FAB shop that offers both ENIG and IAg and see what they like best and what their reasons are. Better yet ask users of IAg and ENIG what they think.
Regards,
George
George M. Wenger (908)-546-4531
Reliability / FMA Engineer
Base Station and Subsystems Group
Andrew Corporation, 40 Technology Drive, Warren, NJ 07059
[log in to unmask]
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Scott Lefebvre
Sent: Wednesday, November 24, 2004 1:43 PM
To: [log in to unmask]
Subject: [TN] Immersion Silver
I just got off the phone with one of our PCB FAB shops and was surprised on his response to Immersion Silver as a solder finish.
He suggested that we do not use it as a replacement for HASL and to use gold instead. All the things I've read and did research on IAg in
contraction to he said. The shop said shelf life is less than 6 months and tarnish was a big issue. It was more expensive than ENIG and not that many shops do it in-house.
My understanding is the shelf life is 6-12 months if stored and handled properly. They silver used today has an anti-tarnishing agents to prevent tarnishing. I was also under the impression that IAg is less costly than ENIG.
Your opinion in this matter would be greatly appreciated.
Thank you,
Scott
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
------------------------------------------------------------------------------------------------
This message is for the designated recipient only and may
contain privileged, proprietary, or otherwise private information.
If you have received it in error, please notify the sender
immediately and delete the original. Any unauthorized use of
this email is prohibited.
------------------------------------------------------------------------------------------------
[mf2]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|