Now Steve...You KNOW the customer is ALWAYS right, except for when we
need to educate them.
First, I would ask the customer WHY the rework is unacceptable.
They may actually have a valid reason.
Next, I would educate them. They may be concerned about flux getting
into the connector. Are you using OA or NC? They may be concerned
about damage to the plated surface. They may be trying to punish you
and teach you to do things right the first time even though we all know
people do make mistakes.
-Carrie
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
Sent: Wednesday, November 24, 2004 12:10 PM
To: [log in to unmask]
Subject: [TN] Samtec PCS2 Socket issue...
Hi All!
First of all, I would like to wish everybody a safe and happy
Thanksgiving!
I have an issue that I would like to bounce off of you all. We're
building an assembly that uses some Samtec "Power Combo Sockets", here's
the *.PDF link to it:
_http://www.samtec.com/ftppub/pdf/PCS2.PDF_
(http://www.samtec.com/ftppub/pdf/PCS2.PDF)
Due to the design of assembly, we had to hand solder these in. The hole
diameter in the board for the power pins of these sockets are .072",
Samtec recommends .058".
We experienced some sockets that had solder flowing up into the power
pin contacts to the point that prevented full insertion of the mating
header, so we removed the solder to allow full insertion using a solder
extractor.
The contacts for the power pins are Tin plated as you can see from
Samtec's drawing, so there really is no contamination from the solder
as there would be with gold plated contacts which the signal pins are
plated with
Now we're being told that our rework was unacceptable, and that the
sockets need to be replaced...I don't see what we did affects the
performance of the socket in any way.
If the mating header can be fully inserted, then electrical contact
should be fine in my opinion. If anything, I feel that the electrical
contact may have been improved slightly due to the tighter fit between
the header pin and the socket contact...it surely isn't degraded.
Am I out in left field about this?
I really appreciate any feedback!
-Steve Gregory-
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|