TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Gebhard.Neifer" <[log in to unmask]>
Date:
Wed, 24 Nov 2004 12:08:48 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Roger Stoops <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
Roger Stoops <[log in to unmask]>
Parts/Attachments:
text/plain (453 lines)
Actually, sounds like ol' Karl may have been thinking of the Scripture that basically says (depending on xlation) 'The spirit is willing, but the flesh is weak' (Jesus, Nisan 14, 33 C.E., Mk 14:38).  But since he also wrote that 'religion is the opium of the people' (something to that effect), he would have had to change "spirit" to "mind" for his philosophy to carry the meaning he intended.

Just thinking out loud.  Sorry if anyone takes offense at the volume.

Roger

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Gebhard.Neifer
Sent: Wednesday, November 24, 2004 11:50 AM
To: [log in to unmask]
Subject: [TN] AW: [TN] AW: [TN] Video analysis of solder joint formation
- NTC


Hats off to you, Ofer!







-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Ofer Cohen
Gesendet: Mittwoch, 24. November 2004 17:38
An: [log in to unmask]
Betreff: Re: [TN] AW: [TN] Video analysis of solder joint formation - NTC

Well, Gerhard, it was indeed written in German, by Karl Marks, in the Communist Manifest.





This statement is a well known example of the limitation of the machines: When the first interpreting machines were developed, this statement was translated into Russian, re-translated into English, and the result was "The Vodka is good, but the meat is rotten".




Ofer




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gebhard.Neifer
Sent: Wednesday, November 24, 2004 18:07
To: [log in to unmask]
Subject: [TN] AW: [TN] Video analysis of solder joint formation




Bob,




in german we have a spoken word which goes like "My mind is willing, only the flesh is weak ..."




Don´t copy David´s penalty performance!




Gebhard




_______________________________

Delphi Deutschland GmbH

Body & Security Electronics

Manufacturing Engineering Design

Albert Einstein Straße 5




D-51674 Wiehl-Bomig




Tel.:         +49 (0)2261-971-880

Fax:         +49 (0)2261-972-880

Mobile:     +49 (0)151-18223504

E-mail: [log in to unmask]        




















-----Ursprüngliche Nachricht-----

Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Bob willis

Gesendet: Mittwoch, 24. November 2004 17:00

An: [log in to unmask]

Betreff: Re: [TN] Video analysis of solder joint formation




Yes you are right; I was trying to be helpful so the forum could look at

this area only. As I run the site I should know this.




I will sort out links separately TOMMOROW; I have to go to soccer practice

now. After watching the David BeckHam DVD I have these new skills to tryout.

Well the mind knows what to do it's the legs I have TO SORT OUT.







Bob Willis

2 Fourth Ave, Chelmsford,

Essex, CM1 4HA, England

Tel: 01245 351502

Fax: 01245 496123

Mobile: 07860 775858

Email: [log in to unmask]

Web: www.leadfreesoldering.com

Web: www.bobwillis.co.uk










-----Original Message-----

From: TechNet [mailto:[log in to unmask]] On Behalf Of Pasquito, Helena

Sent: 24 November 2004 15:34

To: [log in to unmask]

Subject: Re: [TN] Video analysis of solder joint formation




Bob,

I am not able to access the site without a password.




Helena Pasquito




-----Original Message-----

From: TechNet [mailto:[log in to unmask]]On Behalf Of Bob willis

Sent: Wednesday, November 24, 2004 9:12 AM

To: [log in to unmask]

Subject: [TN] Video analysis of solder joint formation







Following a number of emails from TECHNET on video simulations, just though

I would show a few we have featured on the SMART Group web site over the

last few years.




Thanks to Dave Hillman and Doug Pauls for letting me know of the interest at

the SMART Group Conference last week.




RealPlayer is available to download free from a variety of location.




QFP Cracking/Popcorning  BGA Popcorning  PCB Delamination  BGA Solder Short

Inspection

Immersion Testing Components (the Components where in my jacket honest)

Lead-Free Chip Tombstone

Outgassing from Via Holes

Solder Balling During Wave Soldering

Solder Beading During Reflow

Slow Wetting on Surface Mount Pads

Poor Component Solderability

Solder Balling of Solder Paste

Copper Dendrite Growth on PCB

Component Loss on Double Sided Reflow

Outgassing from Solder Mask during Wave Contact

Component Floating on Paste

0201 Chip Component Lifting

Outgassing During Soldering of PTH

Secondary Reflow of Lead-Free Joints




http://www.smartgroup.org/members/defectvid.asp







Have a great thanks giving break over there







Bob Willis




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16

for additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to

[log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to

[log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16

for additional information, or contact Keach Sasamori at [log in to unmask] or

847-615-7100 ext.2815

-----------------------------------------------------




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------




****************************************************************************************




Note: The information contained in this message may be privileged and confidential and thus protected from disclosure. If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you.







****************************************************************************************




---------------------------------------------------

Technet Mail List provided as a service by IPC using LISTSERV 1.8e

To unsubscribe, send a message to [log in to unmask] with following text in

the BODY (NOT the subject field): SIGNOFF Technet

To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)

To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest

Search the archives of previous posts at: http://listserv.ipc.org/archives

Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815

-----------------------------------------------------





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

****************************************************************************************

Note: The information contained in this message may be privileged and confidential and thus protected from disclosure. If the reader of this message is not the intended recipient, or an employee or agent responsible for delivering this message to the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify us immediately by replying to the message and deleting it from your computer. Thank you.


****************************************************************************************

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2