Although I'll hear some in"tents" criticism, I'll mask my inhibitions and
answer anyway.
Since we can tolerate no broken tents at any time, we presently cap the via
on both sides with a dry film Solder Mask, followed by a final cover coat
application of a LPI Solder Mask.
Other people have had success filling the via with a solder mask material or
solder followed by a LPI Solder Mask.
Other people are using a plated-over filled via with or without a final LPI
Solder Mask application.
PWB thickness, the compatibility of the chosen materials, the
filling/plugging process, tolerance for voiding and surface sink will have a
bearing on the acceptability of the process and product for your given end
use environment.
Dewey
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Dee Stover
Sent: Thursday, November 18, 2004 12:52 PM
To: [log in to unmask]
Subject: [TN] plugging vias
Hi all,
Besides the process of tenting vias what other options are available for
plugging vias on a board? Solder? Epoxy? ???? What sort of cost
differences are we talking about.
When using the tenting method have any of you experienced breakage in the
mask barrier, during assembly or rework intervals?
We are experiencing is degradation of the vias that exist under quad
packages after rework. Especially if quad packages are on both sides of
the board, directly over each other. Remove one for rework the flux goes
through the vias and takes up residence under the quad on the opposite side
of the board. Our dunk type ultrasonic cleaner doesn't seem to be able to
wash the flux etc. out from under the quads. We do not work with high
volume of anything so any equipment recommendations should be on the
moderate side.
Any experience on these matters you can pass along will be greatly
appreciated.
Dee Stover [log in to unmask]
Sr. Tech Associate Elect
National Optical Astronomy Observatory
950 N Cherry Ave
Tucson, AZ 85719
www.noao.edu
520-318-8489
FAX 520-318-8303
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|