TECHNET Archives

November 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Wed, 17 Nov 2004 14:03:09 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
From:
"Randy Bock Sr." <[log in to unmask]>
In-Reply-To:
Content-Type:
text/plain; charset="US-ASCII"
MIME-Version:
1.0
Parts/Attachments:
text/plain (149 lines)
Mythological ----bzzzzzzz  swat...

Randy Bock Sr.
Quality Manager
Pitney Bowes
AddressRight Printers
(email)  [log in to unmask]
Newtown Building 2
203 270-4931  Ext
    8-426-4931  In
203 270-4982 Fax




[log in to unmask]
Sent by: TechNet <[log in to unmask]>
11/17/2004 01:49 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
[log in to unmask]


To
[log in to unmask]
cc

Subject
Re: [TN] Strange Soldermask Defect...






It must be huge...


> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Charlie Pitarys
> Sent: Tuesday, November 16, 2004 1:47 PM
> To: [log in to unmask]
> Subject: Re: [TN] Strange Soldermask Defect...
>
>
> I would get a can or RAID and spray your incoming boards!
> On another Wild Kingdom subject, did you know that on average a spider
> is within 7 ft of every human on the planet!!
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: Tuesday, November 16, 2004 3:41 PM
> To: [log in to unmask]
> Subject: [TN] Strange Soldermask Defect...
>
> Hi All!
>
> Well, I've run across some strange problems in my time, but
> this one is
> a new one to me.
>
> I was on the production floor just after lunch, close by one of our
> final inspectors looking at something under her microscope,
> when I hear
> her say; "What the heck is this?" then I hear this big;
> "EWWWWWW!" from
> her...
>
> "Steve! Steve! You gotta' look at this!" she says to me. I pull up a
> chair and peer into the microscope, and I have to say, I've
> never, ever
> seen this before.
>
> Take a look at:
>
> http://www.stevezeva.homestead.com/files/StrangeMaskDefect.jpg
>
> and
>
> http://www.stevezeva.homestead.com/files/StrangeMaskDefectCloseUp.jpg
>
> What should I do? Should I send this to a lab or something? I
> don't know
> what to tell my inspectors, much less explain this to our
> customer...this really tops my list as one of the strangest defects I
> have ever seen.
>
> -Steve Gregory-
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To
> temporarily halt or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=> 4.3.16 for
>
> additional information, or contact Keach Sasamori
> at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with
> following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send
> e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail
> to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives
> Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
> additional information, or contact Keach Sasamori at
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2