Hi Les,
For what it is worth, our high rel customers are not willing to accept
re-balled BGAs unless extensive, long term type reliability testing is
performed 1st to demonstrate that their will not be a problem in the future
and even then it raises many questions. The cost associated with this alone
can be expensive.
joe
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: Tuesday, November 09, 2004 4:39 PM
To: [log in to unmask]
Subject: Re: [TN] Re-balling of BGAs
Hi Les!
There are a number of systems out there for BGA re-balling. Some use
mini-stencils to print paste, or flux on to the BGA, then use a template to
locate
the spheres on to the BGA pads.
Then there is a system that utilizes BGA pre-forms that have the spheres
imbedded into a water-soluble paper for whatever pattern BGA you have that
makes
things pretty easy:
_http://www.winslowautomation.com/bga.asp_
(http://www.winslowautomation.com/bga.asp)
This link will detail to you all the steps that are used to re-ball a BGA.
They also perform this as a service.
That being said, for class 3 product, I would be a little hesitant to use
re-balled BGA's, because of all the thermal cycles that the part is going to
be
subjected to. The first cycle is the intial reflow cycle during assembly.
Then the part is going to be removed, the second cycle. The BGA's pads will
need
to be cleaned-up to remove the old solder so that new spheres can be
attached, a third cycle. The spheres will then need to be attached, a
fourth cycle.
Then the device will have to be attached to the assembly once again, a
fifth
cycle.
I know that with some of the latest Xilinx BGA's where the cost can make
you
cr*p your pants ($2500+), wanting to salvage them becomes a real
consideration. But, with all the thermal cycles that you will be putting
these parts
through during the re-balling and BGA re-attachment process, I would be
hesitant
depending on them during critical applications where their function is
vital.
All the above is for eutectic sphere BGA re-balling. For high lead content
spheres (such as those on Ceramic BGA's), I have no knowledge. I do know
that
the previous link I provided, will direct you to the same re-balling
service
that offers that as well...it's not cheap.
The only time I have re-balled BGA's and used them is with class 2
commercial product... never with class 3.
-Steve Gregory-
November 9, 2004
We have an OEM who has some de-laminated PWA'S with some BGA'S installed.
He wants to salvage the parts and have them re-balled. I have no direct
experience in this area. How does one re-ball a BGA? What types of BGA
can be
re-balled? What are the pros and cons on re-balling? Is this an
acceptable
repair method for Class 3 product?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|