Peter,
I a previous life I did several evaluations of conductive adhesives as a solder replacement. You will find that the adhesive should print as well as solder paste if you double the print speed. Other than for that, it prints the same. I need to qualify it be saying that I did not print fine pitch components, but I don't think this should prove to be a problem. If you want to talk about any other results, I have a few horror stories that I can share.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Peter L
Sent: Friday, November 05, 2004 8:20 PM
To: [log in to unmask]
Subject: [TN] Conductive Adhesive
Hello Technet,
Can someone share their experience on Pros/cons (in particularly process
implication) of applying conductive adhesive Vs solder paste? We have a
request by one customer to investigate conductive adhesive (stencil print
compatible) as a potential substitute for Pb-Sn solder and eventually lead-
free.
Rgds,
Peter
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|