Yes, I agree. All ED copper foils are produced to a 10% tolerance of
these nominal numbers cited. We take discrete measurements of all foil
thickness and these vary little from nominal. I believe the weight
metric was derived from a costing standpoint rather than a thickness; we
merely applied a conversion to allow for verification of the weight
parameter to the circuit thickness which is critical in many
applications.
Jeffrey Bush
Director, Quality Assurance and Technical Support
76 Technology Drive - POB 1890
Brattleboro, Vermont 05302
802.257.4571.21
http://www.vtcircuits.com
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Friday, November 05, 2004 1:54 PM
To: [log in to unmask]
Subject: Re: [TN] copper weight
Hi Jeffrey and all,
Things are not quite as simple as has been portraied--the density of ED
copper is not a fixed number, it varies depending on the plating details
of a given
batch.
This is the reasopn ED Cu foil is given as a weight per area, not as a
fixed
thickness. The situation is further muddies, because many of these foils
have
a variety of adhesion "tooth" geometries.
Thus, to say "copper weights in oz - 1/4, 3/8, 1/2, 1.0, 2.0, 3.0, 4.0
are as
follows in microns - 9, 12, 18, 35, 71, 107, 142" is not correct. The
micron
numbers are only the metric equivalents of the mil numbers, BUT the
mil-thicknesses are only NOMINAL values with significant +/- ranges.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|