The following link presents tabular data on mechanical properties of
tin-lead solders. Temperature at which the data is collected is not
indicated. I do not know if the interest is in 95/5 Pb/Sn solder (common
for flip chip assembly) and 90/10 Pb/Sn (solder columns on ceramic column
grid array packages), or 90/10 Sn/Pb and 95/5 Sn/Pb, as indicated in
Werner's note. In my experience in stud pulling high lead (95-97%) flip and
eutectic tin-lead chip bumps at room temp, the eutectic shows higher tensile
strength. The tabular data also shows this. No data is shown for solders
with greater than 70% Sn.
Regards,
Leo
http://www.efunda.com/materials/solders/tin_lead.cfm
-----Original Message-----
From: Werner Engelmaier [mailto:[log in to unmask]]
Sent: Thursday, October 28, 2004 7:59 AM
To: [log in to unmask]
Subject: Re: [TN] Solder Strength over temperature
Hi Rich,
The tensile strengths of 63/37, 90/10 and 95/5 solder alloys are highly
temperature and strain-rate dependent. I have a graph of tensile strengths
of
near-eutectic Sn/Pb, but not the others. Bet generally, 90/10 and 95/5
solders will
be stronger than near-eutectic alloys.
Wht do you need this info--the strength of properly attached solder joints
is
more than adequate for any strss-producing loading condition--other things
will fail first. This may change with LF-solders.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|