Thanks for the help,
I received the information I need direct from Nelco; and I want to share it.
N4000-13
X axis CTE (-40 to +125C.)
16.9 ppm/°C
Y axis CTE (-40 to +125C.)
4.9 ppm/°C
Z axis CTE (below Tg)
69ppm/°C
Z axis CTE (above Tg)
283ppm/°C
What is interesting is the large anisotropy between x and y. That sure makes
an alternating lay-up scheme important.
Regards,
Werner Engelmaier
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------