one word of caution: do not apply solder at the thermocouple tip. The
resistance of the tip will change and give you false readings.
jk
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Jason Gregory
Sent: Friday, October 22, 2004 11:45 AM
To: [log in to unmask]
Subject: Re: [TN] A poll of sorts...concerning thermocouple attachment
Dr. Zapfardt? Glad it's Friday. :)
Jason Gregory
Manufacturing Engineer
x5593
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of [log in to unmask]
Sent: Friday, October 22, 2004 10:20 AM
To: [log in to unmask]
Subject: Re: [TN] A poll of sorts...concerning thermocouple attachment
My first choice would be to attach TCs using either high-temp solder or
conductive epoxy (after first removing the existing alloy at the
connection). If
you can commit a PCBA to profiling, this is the long-term way to go.
Of course there are times when you cannot sacrifice a PCBA to the Profile
Gods. Temprobes are good (we tested them a number of years ago) as long as
the
point of contact is on the flat of the joint being probed. If you hit it
at
an angle, you can be off by as much as 10 deg C.
Like Karen, I have had pretty good success with aluminum tape. Quick,
cheap
and easy and with very little addition of tolerance. The article on KICs
website explains it pretty well.
According to Dr. Zapfardt in the October issue of Circuits Assembly ("On
The
Forefront")attaching the TC with Kapton tape is for bozos who really are not
interested in actually getting accurate profiles, but are just killing
time.
I couldn't have said it better myself.
Phil Zarrow
ITM Consulting
Durham, NH USA
www.ITMconsulting.org
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|