Hi Victor,
I suspect what you are experiencing is called Halo effect. As you note,
flux residue is the most common cause for this effect. The type of
cleaning solution which will be appropriate is typically and primarily
determined by understanding the type of LF flux you are using. The LF
Flux manufacturer may be able to recommend what type of cleaning
chemistries have demonstrated the ability to work well. Once the
cleaning chemistry is selected; consider the rinsing and drying needs as
well.
The cleaning chemistry suppliers AAT mostly works with are Kyzen,
Petroferm and Zestron chemistries.
Hope this provides an opportunity to be useful information,
Shean R. Dalton
Austin American Technology
www.aat-corp.com <http://www.aat-corp.com>
(+1) 512-335-6400 ext. 20
-----Original Message-----
From: Victor G. Hernandez
Sent: 10/27/2004 7:57 AM
To: [log in to unmask]
Subject: [TN] Lead Free Fluxes
Hello,
Can someone recommend a general purpose LF Flux remover/dissolver?
I need to cross section a Ball Grid Array solder bump in which I want to
minimize the epoxy voiding around the solder ball due to a crystal clear
ring formation residue left from the solder paste. Has any one
conducting BGA cross section ran across this artifact.
Victor,
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|