In the disk drive industry (where costs drive everything), we have found
that we are having very little, if any cost impact using immersion gold -
with much better compatibility and reliability than other processes (for
us). We are about the same stackup as you mention. We also use SAC (Tin
96.5% Silver 3% Copper 0.5%.) Our FR4 has not had heat issues, verify
component capabilities. We use an Electrovert Omniflo 10 oven for PCBA, it
is a 10 Zone oven. Work closely with your suppliers.
Sincerely,
-----------------------------------
Cheryl Johnson, C.I.D.+
Manager
ExcelStor US Office, Engineering Services
Email: [log in to unmask]
Tel: (303) 684-7291
Fax: (303) 684-7268
Mobile: (303) 809-5815
-----------------------------------
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Jowan Iven
Sent: Tuesday, October 26, 2004 4:18 AM
To: [log in to unmask]
Subject: Re: [LF] lead free PCBA inquiry
Hello Leo,
I personally think that your approach is too easy.
Just ask the lead free forum and everything will be presented on a platter.
In the real world it all depends on the application and the process.
So when I answer your questions with the limited info you gave it would look
something like this
1 OSP (only cost perspective)
2 Yes but it depends on how you specify "withstand"
3 A lot of data still has to be gathered, but it is the most common LF alloy
4 no but be carefull, labelling is becoming more important
5 see the web, visit seminars and read books, the LF technology is
constantly evolving.
regards
Jowan Iven
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]] On Behalf Of Leo B. Buya
Sent: dinsdag 26 oktober 2004 12:14
To: [log in to unmask]
Subject: [LF] lead free PCBA inquiry
Hi to all!
I am a PCB layout Engineer and been doing some reading/research for our Lead
Free assembly that includes the PCB, reflow and wave soldering
considerations, components to use and other Lead-free inputs applicable to
attain our Lead-free assembly. We manufacture Digital Enhanced Cordless
Phones. Our PCBs are normally 1.0mm thickness, FR4 (double sided) and sizes
ranges from 70mm x 80mm and above.
My questions are:
1. What can you recommend as the better PCB finish (plating) for such board
(DECT)?
2. Can a FR4 with a Tg of 135ºC withstand the temperature required for
Lead-free and so with our PCB thickness?
3. Is a SnAgCu solder alloy best suited for such board?
4. Is it true that the assembly for lead-free must have separated assembly
area to that of the leaded assembly since contamination can occur?
5. Please provide me any information that are vital for our cross over to
Lead-free environment?
Your inputs are highly acknowledged. Thank you!
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
--------------------------------------------------------------------------
DISCLAIMER:
This e-mail and any attachment(s) sent with it are intended exclusively for
the addressee(s), and may not be used by, opened by, passed on to, or made
available for use to, any person other than the addressee(s). Stork rules
out any and all liabilities resulting from any electronic transmission.
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|