Do you buy from well established BGA makers or from 'other' sources? And what failure rate do you relate to? LM is so big, you are supposed to mount tons of boards yearly, and each failure requires repair, paperwork, reporting and all that annoying stuff, so, as a MIL maker too, we too want see no failures at all. I suppose your frustration relates to a ppm level rather than percentage, i.e. a few defect balls a week in a line that produces hundreds of large boards a week....
We had a brainstorming once about same worry as yours, resulting in a somewhat odd proposal: immerse all incoming BGA packages into -65 (or lower) Centigrade liquid, take them up and give a few mechanical shocks at 1,500 G's. Weak members would fall off. Theoretically correct, but won't be much loved by economists, nor by the incoming inspection.
Xilinx is one of our sources, they seem to understand what we expect from the above standpoint, see for example this page : http://www.xilinx.com/products/qa_data/table2b.htm. And it also seems as they apply what they promise. This said, we don't mean to favourize X. Hope I don't trespass Jack's aesthetic violation laser beam control....
Ingemar Hernefjord
Ericsson Microwave Systems
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of John Perry
Sent: den 18 oktober 2004 21:32
To: [log in to unmask]
Subject: [TN] BGA ball-to-package failures
TechNet Posting on Behalf of Tom Clifford, Lockheed Martin, Sunnyvale
CA:
I'm concerned about incoming BGA ball-to-package integrity. All our
solder-joint-cycle reliability predictions deal with cyclic-fatigue
shear failure thru the solder-joint fillet, top and/or bottom. And,
most t-cycle failures do occur thru the fillet, as anticipated.
However, we have seen, dramatically, that BGA balls can pop right off
the interface at the bottom of the BGA package, in "premature" failure.
Certainly this sort of failure cannot be predicted on fundamental
grounds, or even predicted based on actual test, or compensated for in
our component/PWB selection/design/processing. If the BGA ball is
"weak" at the ball-package interface, all prediction bets are off!!! We
are at the mercy of the supplier and of that particular
part...P/N/...lot...batch. Additionally, the exposure will get worse,
in the hi-rel mil-aero world, as BGA applications increase in number and
consequence, and as supply-chains expand.
I'm thinking the industry (users and supplier/packagers) should do at
least these things:
1)Develop or identify some sort of standard physical test (shear or
tensile) to measure the as-shipped or as-received strength of the
ball-to-package joint, probably room temperature, maybe at an elevated
temperature.
2)Start gathering a data base, linking mean and variability to material
and process.
3)Start relating this relative ball-to-package strength data to maverick
failures at the interface, in t-cycle testing.
4)Depending on results, and if these failures persist in mil/aero
applications, consider adding a suitable qualification and
lot-acceptance test and criteria to incoming BGAs.
Certainly the causes and consequences and fixes will be and probably are
being addressed, but industry recognition of the problem, up-front would
be useful. Perhaps the "problem" has already been solved, but my guess
is that it needs some attention, to help move it way down the list of
reliability concerns.
Comments? Tom Clifford
Mike Green
Production Design Engineering
Dept 7JGS; B157; Col 3D3
Lockheed Martin Space Systems
1111 Lockheed Martin Way
Sunnyvale, CA 94089
office 408-743-1635
Synergy works at LMC. "Show me the data."
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|