I see no reason why hermetically sealed elcos cannot be conformally
coated. If an elco generates pressure, it is because it is already in a
fault condition and should therefore be changed, anyway.
Brian
Lum Wee Mei wrote:
> Hello,
>
> Since we are on electrolytic cap, how about conformal coating (acrylic) on them?
> We have been coating them since day one as no one has instructed that
> electroltic cap cannot be coated.
>
> Recently, there have been opinion that we cannot coat them as there will be no
> gap for the pressure to escape - similar to the below issue?
>
> What are your opinions?
>
> Regards,
> Wee Mei
>
>
> Quoting Brian Ellis <[log in to unmask]>:
>
>
>>It depends on what cleaning medium you are using. If you are using a
>>halogenated solvent and just a microgram penetrates inside the casing,
>>you will see customers complaining of failures after 6 months to 2
>>years. This is well-known and was publicised by Sprague in the 1960s.
>>This company recommended using only hermetically sealed elcos if
>>cleaning in halogenated solvents. They also tested aqueous cleaning and
>>determined zero effect by aqueous cleaning, including with saponifiers
>>which could cause superficial corrosion of the outer case. However,
>>IMHO, it always makes sense with aqueous cleaning to have each stage
>>slightly warmer (say 5 deg C) than the previous one, so that you always
>>have positive pressure inside the cans while they are wet, to prevent
>>the ingress of contaminated water.
>>
>>Brian
>>
>>Scott Lefebvre wrote:
>>
>>
>>>We have a problem with the plastic disk coming off after being process
>>
>>through our In-Line PCB washer. What concerns if any should I have.
>>
>>>---------------------------------------------------
>>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>>To unsubscribe, send a message to [log in to unmask] with following text in
>>>the BODY (NOT the subject field): SIGNOFF Technet
>>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>
>>>To receive ONE mailing per day of all the posts: send e-mail to
>>
>>[log in to unmask]: SET Technet Digest
>>
>>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>
>>for additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-509-9700 ext.5315
>>
>>>-----------------------------------------------------
>>>
>>>
>>
>>---------------------------------------------------
>>Technet Mail List provided as a service by IPC using LISTSERV 1.8e
>>To unsubscribe, send a message to [log in to unmask] with following text in
>>the BODY (NOT the subject field): SIGNOFF Technet
>>To temporarily halt or (re-start) delivery of Technet send e-mail to
>>[log in to unmask]: SET Technet NOMAIL or (MAIL)
>>To receive ONE mailing per day of all the posts: send e-mail to
>>[log in to unmask]: SET Technet Digest
>>Search the archives of previous posts at: http://listserv.ipc.org/archives
>>Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>>for additional information, or contact Keach Sasamori at [log in to unmask] or
>>847-509-9700 ext.5315
>>-----------------------------------------------------
>>
>
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|