TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Peter Swanson <[log in to unmask]>
Date:
Fri, 1 Oct 2004 14:19:29 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
<51858C36CF03D311847F00508B2C40B23D75F0@INTERTRONICS_01>
Content-Type:
text/plain; charset=us-ascii; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (65 lines)
I'm sure you can find some conformal coatings that would meet these
requirements. Many, many, years ago, I sold a two-part flexibilised
(essential) solventless (also essential, or with a reactive solvent)
epoxy that was made exactly for this purpose. I can't even remember the
maker (USA), as senility sets in. It was a low-viscosity dip or spray
product with a 12 hr open time and required, if I remember correctly, a
2 hour cure at about 100 deg C. I do remember the maker said there was
no carbon pigment in it, it was just a heavy dosage of reactive dye.
Maybe Googling will find something?

Brian

Peter Swanson wrote:

> I am looking for ideas for a pcb assembly coating, the function of which is
> to hide the component IDs to prevent piracy and copying. This is a
> non-specific requirement which comes up from time to time.
>
> Basic requirements:
> 1) Opaque - black, but could be any colour I guess
> 2) Fairly permanent and resistant to tampering - leads me to an epoxy type?
> Anything can be removed if you try hard enough, but epoxy would be the
> toughest
> 3) Easily applied, no special equipment - aerosol can? Brush on with fast
> (thermal cure)? Single part?
>
> There's some other factors which would be specific to particular assemblies
> (thermal and electrical characteristics) of course, but I'm just looking for
> something generic at the moment.
>
> Anyone have any ideas or already use something for this purpose?
> TIA,
> Peter
> --
> --------------------------------------------------------
> Peter Swanson           [log in to unmask]
> INTERTRONICS               http://www.intertronics.co.uk
> Tel: +44 1865 842842                Oxfordshire, England
> INTERTRONICS is dedicated to providing quality material,
> consumable and equipment solutions to high technology
> assembly industries, with the highest levels of technical
> support and customer service.
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2