TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Jason Gregory <[log in to unmask]>
Date:
Wed, 27 Oct 2004 16:12:11 +0100
Reply-To:
Subject:
From:
Mike Fenner <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (256 lines)
For the finer particle size a slight reduction in metal percent would be
good, but a finer particle size does not actually address your original
concern of release. Smaller particle sizes are chosen to suit deposit
size/volume. What you would have with the finer size is a more expensive
solder paste with possibly reduced process windows. Suggest it would be
preferable to address your printing concerns with the original formulation.
Alloy choice between Sn62 or Sn63 does not affect print performance.

Regards

Mike Fenner
Indium Corporation

T: + 44 1908 580 400
M: + 44 7810 526 317
F: + 44 1908 580 411
E: [log in to unmask]
W: www.indium.com
Pb-free: www.Pb-Free.com
-----
SMART 6th European Conference, Brighton 16-18 November 2004
www.smartgroup.org/con2004/conference2004.pdf




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jason Gregory
Sent: Wednesday, October 27, 2004 2:42 PM
To: [log in to unmask]
Subject: Re: [TN] Question about 2% Ag and stencil release


Paste was brand new and thoroughly warmed. Metal load on both pastes is
89.5% metal load.



Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)310-7588 cell
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of David Suraski
Sent: Wednesday, October 27, 2004 8:24 AM
To: [log in to unmask]
Subject: Re: [TN] Question about 2% Ag and stencil release


Daan's assessment sounds right. This could have been a paste dry out
issue.

Jason, do you know what the metal % was in each of these solder pastes?


Best regards,
David Suraski
AIM



-----Original Message-----
From: Jason Gregory [mailto:[log in to unmask]]
Sent: Wednesday, October 27, 2004 9:08 AM
To: [log in to unmask]
Subject: Re: [TN] Question about 2% Ag and stencil release

Yes, same flux in both pastes



Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)310-7588 cell
[log in to unmask]



-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Taheri, Kamran
Sent: Tuesday, October 26, 2004 7:39 PM
To: [log in to unmask]
Subject: Re: [TN] Question about 2% Ag and stencil release


Jason, did both solder pastes have the same flux chemistry?

-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Daan Terstegge
Sent: Tuesday, October 26, 2004 4:00 PM
To: [log in to unmask]
Subject: Re: [TN] Question about 2% Ag and stencil release


Hi Jason,

I don't believe this has anything to do with silver.
The fine powder of your type 5 paste has a MUCH larger ratio between
soldersurface and soldervolume than the part 3 type, which means that it
is more difficult to keep the powder particles stable and oxide-free.
The smaller process window increases the chance of printing problems.
Hopefully a more accurate description will be given by one of the paste
manufacturers on this forum, but I think I'm pretty close....

Best regards,

Daan
http://www.smtinfo.net

----- Original Message -----
From: "Jason Gregory" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Tuesday, October 26, 2004 9:44 PM
Subject: [TN] Question about 2% Ag and stencil release


> Has anybody had any experience or seen/written studies involving 2% Ag

> release from stencil apertures? We have a stencil, parts are small
resnets,
> about 15 mil pitch on a .006" thick stencil. Tried 2% silver paste
> (for tombstoning of other parts) with type 5 powder and had major
> release problems. We kept the same parameters on the screen printer
> (for reference/control purposes) and swapped in our "normal" 63/37
> Type 3
powder
> and release issues "virtually" went away. Not all the way, but for the
most
> part. I thought smaller mesh should have meant better release. Solder
> gurus ------- enlighten me!
>
> Jason Gregory
> Manufacturing Engineer
> Innova Electronics
> (281)653-5593
> (281)653-5594 fax
> (281)310-7588 cell
> [log in to unmask]
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
> or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
> -----------------------------------------------------
>
>

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask]
or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2