Steve
There are several products on the market that have properties similar to
prepreg that are designed for via filling and could conceivably be used
for this application. Often the designer fills the via and then uses the
same pad for the BGA attachment site (after overplating) and reduces the
path length to the second layer which is often a ground. Reducing the
path length obviously improves the electrical performance.
Best regards
Lee
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Kelly
Sent: Tuesday, October 26, 2004 3:22 PM
To: [log in to unmask]
Subject: [TN] Filled vias
Good day to all,
We have a customer who wants us to fill some blind vias with pre-preg.
First
I have not heard of a pre-preg fill product. Second the via to be filled
will be .003 - .004 . Third - the customer is under the impression this
will
improve electrical performance- is this true? Any thoughts or help would
be
appreciated. Thanks in advance. Steve Kelly
PFC Flexible Circuits Limited
Ph: (416) 750-8433
Fax: (416) 750-0016
Cell: (416) 577-8433
E-Mail: [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|