Jack the heat generated is almost instantaneous, heat transfer takes
time to reach equilibrium. A 50% duty cycle will heat the trace
instantly but the system will reach a different equilibrium temperature.
-----Original Message-----
From: DesignerCouncil [mailto:[log in to unmask]] On Behalf Of Jack
C. Olson
Sent: Thursday, October 07, 2004 2:35 PM
To: [log in to unmask]
Subject: [DC] Trace Heating
It seems like everyone is asking me questions I can't answer today.
We have been using the thermal trace calculator from UltraCAD
( http://www.ultracad.com/calc.htm )
but today someone asked me how time affects the temperature.
For example, what if the trace is only energized for half a second?
How hot will it get? Or how about a 50% duty cycle?
I can't seem to find any info about it. Anyone have references?
Jack (aka "one hot board designer")
------------------------------------------------------------------------
---------
DesignerCouncil Mail List provided as a free service by IPC using
LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET
DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases
> E-mail Archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
------------------------------------------------------------------------
---------
---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
---------------------------------------------------------------------------------
|
|
|