TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Kaye Clayo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Kaye Clayo <[log in to unmask]>
Date:
Mon, 4 Oct 2004 18:02:53 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (52 lines)
Hi,

I could use some help on a problem.

I recently revised a board and received a prototype quantity to audit from the same vendor that fabs the production boards.
The prototypes that we received are SMOBC/HASL with LPI soldermask and are double-sided smt reflow with manually
soldered through hole parts (same as the previous revision).

On the new prototype run, there is what looks like a slight goldish tint to the exposed tin/lead pads on the board.
When the bare board is viewed under magnification, the solder surfaces look grainy and mottled, not shiny like one would
expect with tin/lead. There is a definite definition where the soldermask border is located around exposed pads, and
the boards do not feel sticky.

So far the boards appear to have soldered just fine in both top side and bottom side reflow operations, using OA water-soluble flux.
The boards are having a problem in the through hole (manual) soldering op, using rosin flux.
The solder joints are very poor, and they have some black stuff bubbling out of the holes.
One engineer scratched off an area of a smt pad on a bare board with a white eraser, and then touched a hot solder
iron to the scratched area and the solder wetted up to the area that was not scratched off.

The vendor says that it is some kind of tarnish that is over the surface and in the holes. They have a few overage boards
still at the fabrication site, and those boards have the same goldish hue.
We received these prototype boards on a 2-week delivery, and began assembling the boards
the day after we received them.

Does anyone have any experience with a problem like this or have any ideas what the problem could be?
I am having some trouble believing that it is tarnish on HASL finish.

Any ideas would be appreciated.

Thanks,

Kaye Clayo
Sr. P. C. Layout Designer


CONFIDENTIALITY NOTE: This message is intended only for the use of the individual or entity to which it is addressed and may contain information that is privileged, confidential, and exempt from disclosure under applicable law. If the reader of this notice is not the intended recipient, you are hereby notified that any dissemination, distribution or copying of this communication is strictly prohibited. If you have received this communication in error, please notify the sender immediately.


_____________________________________________________________________________
Scanned by IBM Email Security Management Services powered by MessageLabs. For more information please visit http://www.ers.ibm.com
_____________________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2