It has a pad (pin number 21) that is underneath and a
note that says: "To maximize the thermal performance
of the LTC3414, the exposed pad should be soldered to
a ground plane."
I built the footprint and made sure the pad was
soldermasked and included the pad shape in the
pastemask file.
The engineer was trouble-shooting and de-soldered the
part from the board. It looks like there was no
solderpaste or solder on the pad.
Here's the (dumb) designer question: How would the
solder get to that pad underneath? Should we add a
requirement note saying that the part should be
inspected or x-rayed to see if the pad is indeed
soldered?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------