TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 29 Oct 2004 17:57:29 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
I was asked what environment these assemblies were going into, and I  told
the lady that these were military assemblies. She then told me that I should
replace them. She also said that although Coil Craft hasn't had any reports,
but if there should be one than more crack i.e., one on each side of the part,
the possibility exists that the case could fall off. We're advising our
customer of this issue since we have shipped product to them.

-Steve Gregory-

Steve,

Was the crack merely cosmetic or is there potential for wire damage with the
 excess potting compound?

Jim Carlson
Reliability/Quality Engineer
Rockwell Collins





---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2