TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Steve Kelly <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Kelly <[log in to unmask]>
Date:
Thu, 28 Oct 2004 15:11:43 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (137 lines)
Thanks everyone. With your help I was able to figure this out. Regards Steve
Kelly

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of David Greig
Sent: Wednesday, October 27, 2004 8:13 AM
To: [log in to unmask]
Subject: Re: [TN] Filled vias

On topic - one way of creating resin filled blind vias is in a sequential
build, whereby the resin from the prepreg bonding the separate drilled
sub-boards squeezes thru the via holes. It is then possible to prepare the
outer surfaces and actually plate over the resin plugs. Useful for via in
pad.

Off topic, via inductance can be approximately modelled as being
proportional to ln(1/radius), smaller vias are more inductive, but at least
you can have more of them.

Best Regards

David Greig
_________________________________________
Director
GigaDyne Ltd
Buchan House
Carnegie Campus
Dunfermline KY11 8PL
United Kingdom
Tel. +44 (0) 1383 62 49 75
_________________________________________


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Jeffrey Bush
Sent: 27 October 2004 12:12
To: [log in to unmask]
Subject: Re: [TN] Filled vias

Smaller vias produce less inductance making low inductance bypass caps more
effective of low inductance no longer needed. The resin fill is a normal
function of the sub-assembly build up technique for blind vias.




Jeffrey Bush
Director, Quality Assurance and Technical Support

                          76 Technology Drive - POB 1890
                             Brattleboro, Vermont 05302-1890
                                Tel. 802.257.4571.21 Fax. 802.257.0011
                                    [log in to unmask]
                              http://www.vtcircuits.com


-----Original Message-----
From: Steve Kelly [mailto:[log in to unmask]]
Sent: Tuesday, October 26, 2004 3:22 PM
To: [log in to unmask]
Subject: [TN] Filled vias

Good day to all,

We have a customer who wants us to fill some blind vias with pre-preg.
First I have not heard of a pre-preg fill product. Second the via to be
filled will be .003 - .004 . Third - the customer is under the impression
this will improve electrical performance- is this true? Any thoughts or help
would be appreciated. Thanks in advance. Steve Kelly



PFC Flexible Circuits Limited

Ph: (416) 750-8433

Fax: (416) 750-0016

Cell: (416) 577-8433

E-Mail: [log in to unmask]




---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please visit
IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
--
Virus scanned by Lumison.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2