Has anybody had any experience or seen/written studies involving 2% Ag
release from stencil apertures? We have a stencil, parts are small resnets,
about 15 mil pitch on a .006" thick stencil. Tried 2% silver paste (for
tombstoning of other parts) with type 5 powder and had major release
problems. We kept the same parameters on the screen printer (for
reference/control purposes) and swapped in our "normal" 63/37 Type 3 powder
and release issues "virtually" went away. Not all the way, but for the most
part. I thought smaller mesh should have meant better release. Solder
gurus ------- enlighten me!
Jason Gregory
Manufacturing Engineer
Innova Electronics
(281)653-5593
(281)653-5594 fax
(281)310-7588 cell [log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------