TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Werner Engelmaier <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 1 Oct 2004 08:48:13 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (32 lines)
Thanks for the help,
I received the information I need direct from Nelco; and I want to share it.
 N4000-13

X axis CTE (-40 to +125C.)
 16.9 ppm/°C

Y axis CTE (-40 to +125C.)
 4.9 ppm/°C

Z axis CTE (below Tg)
 69ppm/°C

Z axis CTE (above Tg)
 283ppm/°C

What is interesting is the large anisotropy between x and y. That sure makes
an alternating lay-up scheme important.

Regards,
Werner Engelmaier

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2