I asked that very question at a seminar last year in Minneapolis. The answer
is very dependant on the type of product you are building. Hi reliability
products will require a different alloy, different PWB materials, and
different assembly techniques, that is why the US industry is still evolving
as we speak.
Patent issues also will play a prevalent part in the selection process.
Dave Chapman
CSI
-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 2004 1:13 PM
To: [log in to unmask]
Subject: Re: [TN] Lead free
Since Japan is almost 100% lead free, what have they chosen as their
best alloy? or Europe?
Just a thought.
Ramon
-----Original Message-----
From: David Bergman [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 2004 1:28 PM
To: Dehoyos, Ramon
Subject: RE: [TN] Lead free
Hi Ramon,
It will be interesting to see what Technet response is to this. My
personal opinion is that the industry is narrowing on the SAC alloy
(Tin/Silver/Copper). I also believe that the SAC 305 (3% Silver 0.5 %
copper, balance tin) will be the leading alloy. There is a significant
amount of R&D work looking at lower temperature alloys including Bismuth
and Zinc, but none of these are mainstream options yet.
Dave
David W. Bergman, CAE
Vice President, Standards, Technology and International Relations
IPC
2215 Sanders Road #250
Northbrook, IL 60062-6135
Phone 847-790-5340 Fax 847-504-2340
Mobile 847-867-1388
email [log in to unmask] www.ipc.org
IPC IS MOVING: On Friday, September 17, IPC will be moving to a new
office location: 3000 Lakeside Drive, Suite 309 S, Bannockburn, IL,
60015. All phone, fax, web and e-mail service will be down from the
close of business on the 16th until Monday, September 20th. The new main
telephone number will be 1-847-615-7100 and the new main fax number will
be 1-847-615-7105. Direct phone numbers are not yet available. A
complete listing of all new direct phone numbers will be available when
confirmed by the phone company at www.ipc.org/move.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, September 08, 2004 12:15 PM
To: [log in to unmask]
Subject: [TN] Lead free
Technetters:
Last time I checked there were more than a dozen different types
of lead free solders. Has the industry chosen the best one? Or is it
still experimenting with different types?
Regards,
Ramon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|