Thanks for posting the photos, Steve.
The photos look like peeling off of overhanging material like Tin - they
don't look like scrubbing debris.
The areas showing the conductors show pronounced grooves across the
conductors.
This remains a puzzle, but my previous indictment of the scrubbing process
coupled with inadequate removal of the tin/lead etchresist are the best choices
for sources until you can tell us more about the samples.
Susan Mansilla
Robisan Lab
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------