if you aren't repairing the damaged soldermask because it's in a non-critical area, you should check to make sure the damage didn't dig into the laminate and expose fibers.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Genny Gibbard
Sent: Wednesday, September 22, 2004 11:00 AM
To: [log in to unmask]
Subject: Re: [TN] Soldermask repair
All right, that tells how to do a repair, but I was wondering whether it was
even necessary to do the repair in areas only involving laminate exposure.
However, I think I may have found the answer in IPC-A-610, 9.2.2. It says
something to the effect that blisters, voids or scratches in solder resist
that do not bridge adjacent conductors are acceptable.
So I think if a soldering or assembly operation accidentally scratches a bit
of soldermask off, but no copper is exposed or damaged in the area, it is ok
to leave it unrepaired. Is this an acceptable interpretation?
-----Original Message-----
From: [log in to unmask] [mailto:[log in to unmask]]
Sent: September 22, 2004 11:22 AM
To: [log in to unmask]; [log in to unmask]
Subject: RE: [TN] Soldermask repair
whoops, lazy fingers. it's 2.4.1
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Genny Gibbard
Sent: Wednesday, September 22, 2004 10:08 AM
To: [log in to unmask]
Subject: [TN] Soldermask repair
All right, here's my first question for you gurus...
Is there an IPC guideline regarding repairing soldermask that may have been
removed from a PCB in an area that has only laminate being exposed?
I guess we are currently repairing soldermask even when no copper has been
exposed.
Would there be any reason to consider continuing to do this?
Thanks.
Genny
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|