TECHNET Archives

September 2004

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Nowland, Russell Howard (Russell)" <[log in to unmask]>
Date:
Mon, 13 Sep 2004 09:28:43 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Morse, Carrie" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
"Morse, Carrie" <[log in to unmask]>
Parts/Attachments:
text/plain (136 lines)
Hi.
Yup -- thru-holes.  

I'd like to thank everyone for providing feedback on this issue.  Looks
like we will need to work with our supplier on this and maybe do some
destructive testing on existing product as we can ID the holes that show
quality issues. If we come to an understanding of the root cause, I'll
publish the info. 

Thanks again,
Carrie

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Nowland, Russell
Howard (Russell)
Sent: Monday, September 13, 2004 9:07 AM
To: [log in to unmask]
Subject: Re: [TN] Blow Holes -- Where the heck does the moisture come
from anyway?

Carrie,

I agree will all the comments.  I am assuming this are through-vias.  I
would just like to add, you have to be somewhat lucky to nail a void in
a cross-section. It just takes one grind to many or one not enough to
miss it.  One thing to look for is drill quality.  Look at the walls of
the drill and plating and if they are rough then there is a potential
for plating or voids within the plating.  This is caused by to many hits
on a bit, the wrong drill speed, etc...



Russell Nowland
Lucent Technologies
Quail Springs Parkway Plaza
14000 Quail Springs Parkway. Suite 300
Oklahoma City, OK 73134
Phone: 405-302-1660
Fax: 405-302-1622
Cell: 405-203-0034
email: [log in to unmask]


-----Original Message-----
From: Lee Parker [mailto:[log in to unmask]]
Sent: Friday, September 10, 2004 2:31 PM
To: [log in to unmask]
Subject: Re: [TN] Blow Holes -- Where the heck does the moisture come
from anyway?


Carrie

If you cross section the vias, remove the solder from the hole and look
at the copper barrels at very high magnification (use and SEM if
possible)you may see pin holes in the copper or glass bundles protruding
into the hole. This coupled with moisture in the dielectric which is
normal can create the mechanism. When the board is quickly heated in
assembly (reflow or wave solder) the moisture is pressurized and flows
out through the pin holes into the barrels blowing the molten solder in
the barrels out onto the board.

Best regards

Lee

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Morse, Carrie
Sent: Friday, September 10, 2004 2:33 PM
To: [log in to unmask]
Subject: [TN] Blow Holes -- Where the heck does the moisture come from
anyway?

Just wondering a few things here at 2:30 on Friday Afternoon:

1.  What else causes Blow Holes at wave on TH comps?  Is it primarily
moisture?
2.  Where does the moisture come from?
3.  Are certain board materials more likely to sponge up the moisture in
the air?
4.  Can hole wall quality play a part in contributing to blow holes?

-Carrie

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2