Your points are well taken, Bill. These regulations are motivated more politically than anything else but they are here to stay. Your ME's are right that the Lead free parts will work fine with Leaded solder, too. If your products are not sold to the EU, they wouldn't be subject to these regulations at this time. That may change in the future, of course, and you may find the price and availability of 63/37 Sn/Pb becoming more difficult as more people convert. I haven't heard anything from the solder suppliers viewpoints as far as plans to produce the old stuff. As for space shuttles and pacemakers, high reliability devices are exempt from the new regulations while research continues into the long term implications of using the no-Leads.
Thank you,
Paul Black
Manufacturing Engineer
Kronos
E-mail: [log in to unmask]
Voice: (978) 947-1520
Fax: (978) 244-0568
www.kronos.com
Improving the Performance of People and Business(tm)
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Brooks,Bill
Sent: Friday, September 10, 2004 6:05 PM
To: [log in to unmask]
Subject: Re: [TN] Lead free
I talked with our ME's here and they inform me that the current process of
using tin/lead solder WILL BE COMPATIBLE with the new 'lead free' parts that
are being manufactured... So why change processes if you don't need to deal
with the EU...?
The ME's say they have real issues with inspecting high temp solder joints
that do not wet or wick like tin/lead solders... I would expect more trouble
with the ductility of other alloys too, so if your surface mount board is
undergoing thermal excursions and getting stressed at the solder joints due
to CTE mismatches the other alloys are more likely to crack due to work
hardening... and less ductility.
How much real research has been done into these alternative alloys? Do you
want to ride in a Space Shuttle with lead free solder joints? Or put a pace
maker in your chest that has lead free solder joints? Are they truly
reliable?
Who's really driving the move to lead free?
I still maintain that leaded car batteries are a much greater threat to the
environment than cell phones with solder on the small parts they carry
inside. Look at how many cars there are that have to change their batteries
every 5 years or less...
Bill Brooks
PCB Design Engineer , C.I.D., C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
http://pcbwizards.com
-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 2004 11:13 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free
Since Japan is almost 100% lead free, what have they chosen as their
best alloy? or Europe?
Just a thought.
Ramon
-----Original Message-----
From: David Bergman [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 2004 1:28 PM
To: Dehoyos, Ramon
Subject: RE: [TN] Lead free
Hi Ramon,
It will be interesting to see what Technet response is to this. My
personal opinion is that the industry is narrowing on the SAC alloy
(Tin/Silver/Copper). I also believe that the SAC 305 (3% Silver 0.5 %
copper, balance tin) will be the leading alloy. There is a significant
amount of R&D work looking at lower temperature alloys including Bismuth
and Zinc, but none of these are mainstream options yet.
Dave
David W. Bergman, CAE
Vice President, Standards, Technology and International Relations
IPC
2215 Sanders Road #250
Northbrook, IL 60062-6135
Phone 847-790-5340 Fax 847-504-2340
Mobile 847-867-1388
email [log in to unmask] www.ipc.org
IPC IS MOVING: On Friday, September 17, IPC will be moving to a new
office location: 3000 Lakeside Drive, Suite 309 S, Bannockburn, IL,
60015. All phone, fax, web and e-mail service will be down from the
close of business on the 16th until Monday, September 20th. The new main
telephone number will be 1-847-615-7100 and the new main fax number will
be 1-847-615-7105. Direct phone numbers are not yet available. A
complete listing of all new direct phone numbers will be available when
confirmed by the phone company at www.ipc.org/move.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, September 08, 2004 12:15 PM
To: [log in to unmask]
Subject: [TN] Lead free
Technetters:
Last time I checked there were more than a dozen different types
of lead free solders. Has the industry chosen the best one? Or is it
still experimenting with different types?
Regards,
Ramon
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|