True enough. BUT in many cases the manufacturer has no control on where an end user takes the product (e.g. handheld device) and try telling a designer (even if there are in-house design rules) that he/she can't design at the bleeding edge with Angstrom spacing and 500,000 V (hyperbole of course).
Bev
-----Original Message-----
From: John Burke [mailto:[log in to unmask]]
Sent: September 1, 2004 9:07 AM
To: '(Leadfree Electronics Assembly Forum)'; Bev Christian
Subject: RE: [LF] lead-free PCB source
You actually should design to avoid CAF rather than just choosing a
material. CAF formation is hole to plane distance dependent, varies with the
voltage potential on that plane, and is also humidity dependent on the
working environment that it is put into.
John
-----Original Message-----
From: Leadfree [mailto:[log in to unmask]]On Behalf Of Bev Christian
Sent: Wednesday, September 01, 2004 6:06 AM
To: [log in to unmask]
Subject: Re: [LF] lead-free PCB source
Dear SF,
Your question is extremely broad and I am surprised that you have not sought
out experts in your company that know an incredible amount about this
subject.
In terms of finish ENIG, immersion tin, immersion silver, OSP, HASL (Non
lead containing) and others all work WITHIN CERTAIN MANUFACTURING AND
RELIABILITY CONSTRAINTS. We can't help you without knowing more about your
product.
Any decent PCB manufacturer should be able to offer you one or more of these
finishes on PCBs with higher Tg values. But as the British NPL and others
have shown, higher Tg is not enough to stop the potential for conductive
anodic filament growth.
I think you have a lot of homework to do.
sincerely Bev Christian
Research in Motion
-----Original Message-----
From: No Name [mailto:[log in to unmask]]
Sent: September 1, 2004 5:33 AM
To: [log in to unmask]
Subject: [LF] lead-free PCB source
Hello everyone,
Would someone pls recommend PCB suppliers and surface finish for lead-free
PCB fabrication? Thanks for your help.
Regards,
SF
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
---
----------------------------------------------------------------------------
---Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send:
SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
---
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-------------------------------------------------------------------------------
|