DESIGNERCOUNCIL Archives

September 2004

DesignerCouncil@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
George Patrick <[log in to unmask]>
Reply To:
(Designers Council Forum)
Date:
Fri, 10 Sep 2004 15:29:38 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (147 lines)
As usual, politics is king. The EU may be new as a political body, but the
politicians  involved with it have had centuries to develop their craft in
their individual countries.

Make people think you are doing something without doing any real research...

This has been beaten to death, the EU is not going to change their minds
just because it's silly.  And don't hold your breath, I would not be
surprised to see Oregon or Vermont enact similar legislation :)

--
George Patrick
Tektronix, Inc.
Central Engineering, PCB Design Group
P.O. Box 500, M/S 39-512
Beaverton, OR 97077-0001
Phone: 503-627-5272         Fax: 503-627-5587
http://www.tektronix.com    http://www.pcb-designer.com

It's my opinion, not Tektronix'



-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Brooks,Bill
Sent: Friday, September 10, 2004 15:05
To: [log in to unmask]
Subject: Re: [TN] Lead free


I talked with our ME's here and they inform me that the current process of
using tin/lead solder WILL BE COMPATIBLE with the new 'lead free' parts that
are being manufactured... So why change processes if you don't need to deal
with the EU...?

The ME's say they have real issues with inspecting high temp solder joints
that do not wet or wick like tin/lead solders... I would expect more trouble
with the ductility of other alloys too, so if your surface mount board is
undergoing thermal excursions and getting stressed at the solder joints due
to CTE mismatches the other alloys are more likely to crack due to work
hardening... and less ductility.

How much real research has been done into these alternative alloys? Do you
want to ride in a Space Shuttle with lead free solder joints? Or put a pace
maker in your chest that has lead free solder joints? Are they truly
reliable?

Who's really driving the move to lead free?

I still maintain that leaded car batteries are a much greater threat to the
environment than cell phones with solder on the small parts they carry
inside. Look at how many cars there are that have to change their batteries
every 5 years or less...



Bill Brooks
PCB Design Engineer , C.I.D., C.I.I.
Tel: (760)597-1500 Ext 3772 Fax: (760)597-1510
http://pcbwizards.com


-----Original Message-----
From: Dehoyos, Ramon [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 2004 11:13 AM
To: [log in to unmask]
Subject: Re: [TN] Lead free

        Since Japan is almost 100% lead free, what have they chosen as their
best alloy? or Europe?
        Just a thought.
        Ramon

-----Original Message-----
From: David Bergman [mailto:[log in to unmask]]
Sent: Wednesday, September 08, 2004 1:28 PM
To: Dehoyos, Ramon
Subject: RE: [TN] Lead free


Hi Ramon,

It will be interesting to see what Technet response is to this.  My
personal opinion is that the industry is narrowing on the SAC alloy
(Tin/Silver/Copper).  I also believe that the SAC 305 (3% Silver 0.5 %
copper, balance tin) will be the leading alloy.  There is a significant
amount of R&D work looking at lower temperature alloys including Bismuth
and Zinc, but none of these are mainstream options yet.

Dave


David W. Bergman, CAE
Vice President, Standards, Technology and International Relations
IPC
2215 Sanders Road #250
Northbrook, IL 60062-6135
Phone 847-790-5340 Fax 847-504-2340
Mobile 847-867-1388
email [log in to unmask]      www.ipc.org


IPC IS MOVING:  On Friday, September 17, IPC will be moving to a new
office location:  3000 Lakeside Drive, Suite 309 S, Bannockburn, IL,
60015.  All phone, fax, web and e-mail service will be down from the
close of business on the 16th until Monday, September 20th. The new main
telephone number will be 1-847-615-7100 and the new main fax number will
be 1-847-615-7105.  Direct phone numbers are not yet available.  A
complete listing of all new direct phone numbers will be available when
confirmed by the phone company at www.ipc.org/move.

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Dehoyos, Ramon
Sent: Wednesday, September 08, 2004 12:15 PM
To: [log in to unmask]
Subject: [TN] Lead free

        Technetters:
        Last time I checked there were more than a dozen different types
of lead free solders. Has the industry chosen the best one? Or is it
still experimenting with different types?
        Regards,
        Ramon

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------

---------------------------------------------------------------------------------
DesignerCouncil Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF DesignerCouncil.
To temporarily stop/(restart) delivery of DesignerCouncil send: SET DesignerCouncil NOMAIL/(MAIL)
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2