One for discussion I think.
There appears to be limited options when it comes to the control of moisture
sensitive devices through the assembly process, the options being a
paperwork based system or the use of RF tracking software. We have some
ideas here based on the use of indicator strips which change colour when
exposed to moisture. If these were developed to be time sensitive with the
use of an absorbent film of some kind then they could be used to monitor
floor life on batches of components - trays or reels.
For instance, a level 3 strip would change colour (from green to red would
be nice !) after 7 days at a certain humidity. This would have to be based
on J-STD-033. Sounds feasible but I can not seem to trace anyone who is
selling such an item. Does anyone have any experience of this technique
being used ? If not, any comments would be appreciated. Perhaps a good
buisness idea for someone considering the potential market !
Thanks
Bryan Kerr
Principal Quality Engineer
Process and Materials Laboratory
AMS Hillend
Scotland
********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|