What would you recommend to replace connectors?
Re,
Ken Patel
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Charles Caswell
Sent: Tuesday, September 07, 2004 10:18 AM
To: [log in to unmask]
Subject: Re: [TN] Samtec connectors v/s Reworking them
We use our Sniper hot air rework station. Tried it with irons, too much time
and risk.
-----Original Message-----
From: Ken Patel [mailto:[log in to unmask]]
Sent: Friday, September 03, 2004 2:02 PM
To: [log in to unmask]
Subject: [TN] Samtec connectors v/s Reworking them
Importance: High
All,
We use the following Samtec connectors. I have a question for those who use
these connectors on their boards. How do you rework them including removal?
Do you need BGA type nozzle or using soldering iron?
240 pins with 11mm stack height
QTH-120-03-F-D-A
QSH-120-01-F-D-A
240 pins with 8mm stack height
QTH-120-02-F-D-A
QSH-120-01-F-D-A
240 pins with 5mm stack height
QTH-120-01-F-D-A
QSH-120-01-F-D-A
180 pins with 8mm stack height
QTH-090-02-F-D-A
QSH-090-01-F-D-A
Re,
Ken Patel
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|