Sorry Jim, but I respectfully disagree.
I want my engineering info straight. From what Nelco gives me, I cannot
determine the thermal expansion from 25 to 230C, from 0 to 180C or anything other
than 50 to 260C--that is simply not acceptable and lousy technical information
to boot.
We certainly understand the impact of Tg, but
Why not give CTE values below and above Tg; that way everybody can determine
what they need. While, of course, the thermal expansion to soldering
temperatures is important for the reliability of the PCB interconnect structures, it
is not enough for the more severe environments like those for military and
automotive products. This is particularly important in the z-axis, since that
determines the loads on both the Cu barrel and the innerlayer connections to the
barrel.
Regards,
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 386-437-8747, Fax: 386-437-8737, Cell: 386-316-5904
E-mail: [log in to unmask], Website: www.engelmaier.com
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|